Hastelloy C-22 Pipe Description

The main elements of Hastelloy C22 pipe include cobalt, chromium, tungsten, molybdenum and small amounts of aluminum, titanium and nitrogen. Cobalt element improves the strength and hardness of the alloy, chromium element has an important impact on the corrosion resistance of the alloy, tungsten and molybdenum can increase the high-temperature strength of the alloy. Moreover, the addition of aluminum and titanium elements can refine the grains and improve the toughness of the alloy, while the addition of nitrogen can improve the strength and corrosion resistance of the alloy. Besides, it has good plasticity and toughness and can work with both cold and hot processing. Hastelloy C22 pipe also features excellent oxidation resistance and creep resistance at high temperatures. Hastelloy C22 pipes are commonly used in aerospace, chemical industry, petroleum and other fields because of its excellent corrosion resistance and high temperature strength.

Product Parameters

Product NameHastelloy C-22 Pipe
Outer DiameterRound Pipe4mm-200mm
Square Pipe10*10mm-100*100mm
Rectangular Pipe10*20mm-50*100mm
Wall Thickness0.6mm-6.0mm
Length1-6 meters, Length can be customized
StandardASTM, AISI, JIS, GB, DIN, EN, etc.
SurfaceBlack, Bright Polished, Rough Turning, Matt Surface Treatment, No.4, BA, etc.
CertificateISO, SGS, BV
Production TechnologyHot Rolling, Cold Rolling

Chemical Composition

CSiPSVCrMnFeCoNiMoW
0.015 max0.08 max0.02 max0.02 max0.35 max20.0 – 22.50.50 max2.0-6.02.5 maxRemainder12.5 – 14.52.5 – 3.5

Mechanical Properties

Tensile Strength (ksi)0.2% Yield Strength (ksi)Elongation% in 2 inches
1004545

Physical Performance

 UnitsTemperature in°C
Density8.69 g/cm³24°C
Specific Heat0.093 Kcal/kg.C52°
Melting Range1357-1399°C
Modulus of Elasticity205.5 KN/mm²
Electrical Resistivity113.7 µΩ.cm24 °
Coefficient of Expansion12.4 µm/m °C24-93°
Thermal Conductivity10.1 w/m-° K48°

Scope of Application

C- 276 alloy is used in pesticide production, phosphoric acid production, pickling system, plate heat exchanger, selective leaching system, SO2 cooling tower, sulfonation system, shell and tube heat exchanger, surfacing welding valve, etc.ons, for example, chemical processing, pollution control, pulp and paper production; industrial and municipal waste treatment and acid natural gas recovery.

MESSAGE:
*
Submitting….
Submission successful!
Submission failed! Please try again later
Email error!
Phone error!
Expand more!